Free CWI Practice Questions: The 20-Question Sample, Readable

These are the twenty questions in this program’s free sample, presented readably so you can work them here before you take the sample in the course player. Work each question before reading its answer.

THE PROGRAM IN NUMBERS
Fresh
FULL-LENGTH PRACTICE EXAMS
Drawn new for every attempt from the full question bank
Quick
QUICK PRACTICE
Short mini-quiz drills inside the course
20
FREE SAMPLE QUESTIONS
Try the program before you buy
6 months
OF ACCESS
Full access from the day you enroll

What the sample covers, stated as served: all twenty sample questions are drawn from Part A – Fundamentals content areas — the sample as built samples Part A only. It does not include Part B or Part C questions, and it should not be read as a miniature of all three parts. Parts B and C are covered in the full program and on our worked-question pages: Part B – inspection and flaws and Part C – qualification, fabrication and inspection. The sample’s mix is 5 easy, 7 medium, 5 hard and 3 stretch questions, all on exam content.

AWS publishes the passing standard in its own words: “Candidates must achieve a minimum score of 72% on each exam part to obtain the CWI credential.” There is no averaging across parts — each part is passed on its own line.

1. Two plates meet at their edges to form an L shape for the corner of a box. Which term names this joint?

A. A lap joint

B. A tee joint

C. An edge joint

D. A corner joint

Correct: D. A corner joint joins two members at right angles at their edges, as at the corner of a box. A tee joint involves one member meeting the flat surface of the other instead.

2. At the end of a bead, where the arc was broken, a shallow bowl-like depression remains in the weld. That depression is called a:

A. Keyhole

B. Puddle mark

C. Crater

D. Dimple pass

Correct: C. A crater is the depression at the end of a weld bead where the arc was terminated. Unfilled craters shrink and crack, so proper technique fills the crater before breaking the arc.

3. A weld contains a crack, and the applicable standard prohibits cracks of any size. Because it makes the weld rejectable, the crack is classified as a:

A. Benign discontinuity

B. Cosmetic indication

C. Defect

D. Relevant artifact

Correct: C. A defect is a discontinuity that exceeds the acceptance criteria of the governing standard and renders the weld rejectable. Cracks are prohibited outright in most structural standards.

4. On an adjustable alternating-current gas tungsten arc power source, shifting more of the cycle to electrode positive will generally increase which effect?

A. Cleaning action on the work surface, with more heat into the tungsten and less penetration

B. Penetration with no effect on the tungsten

C. Wire feed speed from the feeder

D. Flux melting in the joint

Correct: A. More electrode-positive time strengthens oxide cleaning but dumps more heat into the tungsten and reduces penetration, while more electrode-negative time does the opposite by heating the work more deeply.

5. A shop proposes eddy current testing on a glass-reinforced plastic tank seam. Why will the method not work on that seam?

A. The seam is too smooth for a probe to follow

B. The seam is above room temperature

C. Plastic reflects ultrasound too strongly

D. Eddy currents can only be induced in electrically conductive materials

Correct: D. Eddy current testing depends on inducing circulating electrical currents in the part, which requires an electrically conductive material such as a metal. Nonconductive plastics cannot support the induced currents the method measures.

6. A single-bevel preparation is cut at 30 degrees measured from a line perpendicular to the plate surface, on one member only. The 30-degree figure describes the:

A. Included groove angle

B. Work angle

C. Travel angle

D. Bevel angle

Correct: D. The bevel angle is the angle between the prepared edge of one member and a plane perpendicular to its surface. The groove angle is the total included angle between both groove faces.

7. A procedure requires fusion through the entire thickness of the joint, with weld metal completely filling the groove from face to root. This condition is known as:

A. Partial joint penetration

B. Intermittent welding

C. Seal welding

D. Complete joint penetration

Correct: D. Complete joint penetration means the weld metal fully penetrates the joint thickness with complete root fusion. Partial joint penetration intentionally leaves part of the joint unfused.

8. A visual examination is planned in a shadowed corner of a fabrication shop where the inspector can barely read a gauge. What must be corrected before the examination can be trusted?

A. Adequate illumination must be provided at the examination surface

B. The weld must be painted before it is examined

C. The examination must be done from farther away

D. Only a mirror may be used in shadowed areas

Correct: A. Visual examination depends on the inspector actually seeing fine surface detail, so adequate light at the surface is a basic precondition. Examining in poor light makes small cracks and shallow undercut easy to miss.

9. During a pipe test, the pipe is turned on rollers so the welder always welds near the top while the joint rotates under the arc. Which position does this represent?

A. 1G, the flat rotated pipe position

B. 5G, because the pipe is horizontal

C. 6G, because pipe is round

D. 4G overhead plate

Correct: A. When the pipe rotates and welding stays in the flat position at the top, the test is the rotated flat pipe position. The welder does not have to change body position around a fixed joint.

10. Before joining a dissimilar-metal joint, a layer of compatible weld metal is deposited on one joint face and then welded to. What is this layer called and why is it used?

A. Buttering, used to provide a transition surface that makes the final joint weldable and sound

B. Tacking, used only to hold parts during fit-up

C. Gouging, used to remove defective metal

D. Sealing, used only to stop leaks visually

Correct: A. Buttering coats a joint face with a layer that is metallurgically compatible with both sides, easing dissimilar-metal joining and sometimes limiting dilution or cracking in the final weld.

11. Before using a gauge to measure weld dimensions on an acceptance check, the inspector notices its calibration sticker shows a past-due date. What should the inspector do?

A. Use the gauge anyway because mechanical gauges do not drift

B. Borrow the welder personal gauge without checking its status either

C. Set that gauge aside and use equipment with current calibration for the acceptance measurements

D. Measure by eye and record the gauge number on the report

Correct: C. Acceptance measurements must come from equipment with current calibration so the recorded values can be trusted. Recording a gauge that was not actually used would misstate how the measurement was made.

12. Above a fillet weld symbol, a curved line bowed outward away from the symbol is drawn touching the top of the triangle. What finished weld face does this contour symbol require?

A. A flush face even with the symbol outline

B. A concave face dished inward

C. No requirement; contour symbols describe the groove only

D. A convex face bulging outward

Correct: D. An outward-bowed contour line calls for a convex weld face, an inward-curved line calls for concave, and a straight line calls for a flush face. The contour symbol is placed with the weld symbol on the reference line.

13. The face of a fillet weld bulges outward with excess metal rather than lying flat or slightly concave. The maximum distance from the face to a line between the toes describes the weld’s:

A. Convexity

B. Concavity

C. Throat size

D. Leg size

Correct: A. Convexity is the maximum distance from a convex weld face to the line joining the weld toes. Concavity is the corresponding measurement for a face curving inward.

14. At the junction where the arrow meets the reference line, a small circle is drawn around the joint of the two lines. No other supplementary symbol is present. What does the circle instruct?

A. The weld is to be made in the shop only

B. The weld requires radiographic examination around the joint

C. The weld extends all the way around the joint

D. The weld is a plug weld through a round hole

Correct: C. A circle at the arrow-to-reference-line junction is the all-around symbol, meaning the weld continues around the entire joint. A flag at that junction, by contrast, denotes a field weld.

15. A gas metal arc weld runs at 28 volts and 250 amperes with a travel speed of 10 inches per minute. Using heat input = volts × amperes × 60 ÷ travel speed in inches per minute, what is the heat input?

A. 42.0 kilojoules per inch

B. 70.0 kilojoules per inch

C. 25.2 kilojoules per inch

D. 4.2 kilojoules per inch

Correct: A. Heat input = 28 × 250 × 60 ÷ 10 = 420,000 ÷ 10 = 42,000 joules per inch, or 42.0 kilojoules per inch.

16. A vessel filled completely with water is pressurized above its operating pressure and held while joints are examined for weeping. Beyond leak detection, what does this hydrostatic test demonstrate?

A. The electrical conductivity of the shell

B. The magnetic permeability of the welds

C. The internal soundness of every weld pass

D. The pressure-containing strength and integrity of the vessel under load

Correct: D. A hydrostatic test loads the whole vessel with pressure, demonstrating overall strength and tightness under conditions beyond normal service. It does not characterize individual weld passes, conductivity, or permeability.

17. A constant-voltage wire welding station shows voltage set correctly at the source but the arc behaves as if voltage at the arc is low. Long, undersized leads are found in the circuit. What is the likely problem?

A. Too much inductance stored in the shielding gas

B. Voltage drop in the welding circuit from excessive or undersized cable length

C. The wire classification is expired

D. The contact tube is too new

Correct: B. Long or undersized welding cables add resistance that drops voltage along the circuit, so the arc receives less than the voltage set and displayed at the power source.

18. At the point where a welder stopped and broke the arc, a small star-shaped crack is found in the depression left at the end of the bead. This is most likely a:

A. Longitudinal crack

B. Underbead crack

C. Crater crack

D. Toe crack

Correct: C. A crater crack forms in the depression left when the arc is terminated without filling the crater, often with a star-like pattern. It is located in the crater itself, not along the toe or beneath the bead.

19. A low-alloy steel containing chromium and molybdenum is scheduled for welding with the same thickness and joint as a mild steel job that needed no preheat. Why does the alloy steel typically require preheat anyway?

A. Alloy steels melt at twice the temperature of mild steel

B. Alloying elements make the steel nonmagnetic

C. Alloying elements raise hardenability, so the heat-affected zone can harden and crack without heat control

D. Alloy steels cannot be welded with standard processes

Correct: C. Chromium, molybdenum, and similar elements increase hardenability, meaning even moderate cooling rates can produce hard heat-affected zones in alloy steels, so preheat and controlled cooling become necessary at thicknesses where mild steel welds easily. Such steels are routinely welded with the standard arc processes.

20. Visual examination reveals a faint, tight linear indication that could be a surface crack or could be a tool mark, and the distinction decides acceptance. What is the most appropriate next examination step?

A. Accept the weld without further checks

B. Measure the weld size again with a fillet gauge

C. Apply a surface method such as liquid penetrant or magnetic particle examination to confirm the indication

D. Grind the area deeply until the question disappears

Correct: C. When visual examination leaves a crack-like indication uncertain, a surface examination method sensitive to fine cracks can confirm whether a real surface break exists. Grinding first would destroy the evidence and may not remove a real crack fully.

Ready to take the sample as a scored quiz? Take the free 20-question CWI sample in the course player. The full program — 1,500 original questions across all three parts and all 21 B5.1 content areas, 21 area drills and a full timed Part A simulation — is the AWS Certified Welding Inspector (CWI) Exam Prep course; read the AWS CWI exam guide for the format and eligibility in full, or enroll for $79 with 6 months of access.

Disclaimer

PassProfessor is an independent exam-preparation provider. This program is exam preparation only: it is not the real exam, it provides no education credit, and completing it does not by itself qualify you for any license or certification. The real exam is run by its own exam body — you register for it, pay its fees, and sit it through that body, not through PassProfessor. All practice questions in this program are original; they are not actual exam questions.