Part A – Fundamentals is the breadth examination: 165 questions presented (150 scored plus 15 unscored pretest questions) in 135 minutes, closed book, at a Prometric test center. Its three heaviest content areas under AWS B5.1 are Definition and Terminology (minimum 12%), Welding Processes (minimum 12%) and Symbols – Welding and NDE (minimum 10%). These ten worked questions drill exactly those three areas.
AWS publishes the passing standard in its own words: “Candidates must achieve a minimum score of 72% on each exam part to obtain the CWI credential.” There is no averaging across parts — each part is passed on its own line.
1. To ensure sound metal at the root of a double-sided groove weld, a welder removes metal from the back side of the joint down to sound weld metal before welding that side. This operation is:
A. Backwelding
B. Backgouging
C. Grooving
D. Scarfing the face
Correct: B. Backgouging is the removal of weld and base metal from the root side to create a sound groove before welding the second side. Backwelding deposits a weld at the root rather than removing metal.
2. The portion of a completed weld that was melted and solidified, consisting of a mix of deposited filler and melted base metal, is referred to as:
A. The heat-affected zone
B. The dilution band
C. The parent metal
D. Weld metal
Correct: D. Weld metal is the metal in a weld that has been melted and solidified, whether from filler, base metal, or both. Parent metal is the unmelted material being joined.
3. A groove weld intended to penetrate the full thickness shows an unfused portion remaining at the root. This condition is termed:
A. Incomplete fusion of the face
B. Root concavity
C. Incomplete joint penetration
D. Excess reinforcement
Correct: C. Incomplete joint penetration occurs when weld metal does not extend through the full joint thickness as intended. The unfused region sits at the root rather than at a groove sidewall.
4. A bright, dense spot on a radiograph of a gas tungsten arc weld indicates a fragment of the nonconsumable electrode became trapped in the deposit. This is a:
A. Slag inclusion
B. Tungsten inclusion
C. Porosity cluster
D. Copper inclusion
Correct: B. A tungsten inclusion is a fragment of the tungsten electrode embedded in the weld metal, typically from dipping the electrode in the pool. Its high density makes it appear bright on a radiograph.
5. A trainee keeps touching the tungsten to the weld pool while gas tungsten arc welding stainless tube. The inspector should expect which discontinuity to appear in the deposit?
A. Slag inclusions
B. Tungsten inclusions
C. Heavy spatter deposits
D. Flux entrapment lines
Correct: B. Touching the tungsten to the pool breaks off fragments that become tungsten inclusions in the weld; the electrode should be removed and reground. Gas tungsten arc welding uses no flux, so slag and flux defects do not occur with it.
6. In arc stud welding, what happens immediately after the stud is lifted to draw the arc and the preset arc time elapses?
A. The stud is withdrawn and discarded
B. The operator strikes the stud repeatedly to forge it
C. The stud is plunged into the molten pool on the work surface
D. Flux is poured over the joint by hand
Correct: C. The stud gun draws an arc to melt the stud end and the work surface, then plunges the stud into the molten pool where it solidifies as a welded fastener.
7. Switching a gas metal arc welding procedure from an argon-rich mix to straight carbon dioxide will most noticeably do what?
A. Eliminate spatter entirely and allow spray at very low current
B. Increase spatter and produce a deeper, narrower penetration profile with a harsher arc
C. Make the tungsten electrode last longer
D. Remove the need for a wire feeder
Correct: B. Straight carbon dioxide gives a harsher arc with more spatter and deeper, narrower penetration, and it prevents true axial spray transfer. Argon-rich mixtures give a smoother arc and support spray transfer.
8. A symbol shows a small circle with an X through it placed below the reference line, and the arrow points to a plate surface where headed fasteners are to be attached. Which weld does this represent?
A. A resistance spot weld
B. A stud weld
C. A plug weld left unfilled
D. A surfacing weld pattern
Correct: B. The circle with an X below the reference line is the stud weld symbol, placed on the side where studs are to be attached, with stud size and spacing dimensioned as needed.
9. A double-groove weld symbol is modified so that a small rectangle is drawn inside the groove shape itself, sitting in the root area between the two prepared members. The tail of the symbol gives a material and a thickness for that rectangular piece. What does the rectangle inside the groove require?
A. A backing bar placed behind the root on the far side of the joint
B. A spacer member placed in the root of the joint, made of the material and dimensions given in the tail or on the drawing
C. A consumable insert that must fuse completely into the root pass
D. A root opening equal to the height of the rectangle, with nothing placed in the joint
Correct: B. A rectangle drawn within the groove symbol designates a spacer placed in the joint root, and its material and dimensions are supplied in the tail or on the drawing. Backing is shown by a rectangle on the opposite side of the reference line from the groove, not inside the groove shape.
10. A connection detail carries a small flag or pennant shape at the junction of the arrow and the reference line. A crew planning shop work asks what that mark means for where the weld is made. What is the correct explanation?
A. The weld may be made wherever is cheapest
B. The weld must be made only in the shop
C. The weld is to be made at the erection site, not in the shop
D. The weld requires a field radiograph before acceptance
Correct: C. The flag at the arrow junction is the field-weld symbol. It designates a weld to be made at the site during erection rather than in the fabrication shop.
Keep going: the full program — 1,500 original questions across all 21 B5.1 content areas, 21 area drills and a full timed Part A simulation — is the AWS Certified Welding Inspector (CWI) Exam Prep course. Read the AWS CWI exam guide for the format, eligibility and passing standard in full, try the free 20-question sample, or enroll for $79 with 6 months of access.
Disclaimer
PassProfessor is an independent exam-preparation provider. This program is exam preparation only: it is not the real exam, it provides no education credit, and completing it does not by itself qualify you for any license or certification. The real exam is run by its own exam body — you register for it, pay its fees, and sit it through that body, not through PassProfessor. All practice questions in this program are original; they are not actual exam questions.